PET

Guichon manufactures valves specially adapted to the production of PET :

Multiways valve, Injection valve, Tank bottom valve

Three-way lift plug valve
Type : 321

DN 1/2" to 6" Class 150 to 2500 Lbs
– Fully jacketed
– Lift plug for friction free rotation
– Stainless steel or special alloys
Three-way piston valve
DN 4" x 4" x 4" Class 2500 Lbs
– Stainless steel body and heating jacket
– Electric actuators (on-off and control service)
– 316L stainless steel

Three-way piston valve
DN 3"x 2" Class 600 Lbs
– Additional side mounted sampling or injection valves
– Manual gear operators

Construction

  • Construction materials: Carbon Steel (CS), Stainless Steel (SS), Duplex & Super Duplex, Titanium, Zirconium, Uranus® B6, Tantalum, Nickel, Hastelloy®, Monel
  • Construction methods: Fabricated (Welded), Cast, Solid

Uses

  • Service conditions: High pressure, High temperature, Low temperature, Abrasion, Corrosion, High viscosity, Vacuum, Reliability, Low acoustic signature, Dead space free
  • Types of fluids: Liquids, Liquids with solid particles, Gas, Powder and powdery media, High viscosity fluids

FAQ - PET

PET – Uses of PET :

– la fabrication de bouteilles, flacons recyclables
– Fibres textiles dites polaires
– Rembourrage de peluches, de coussins

Posted in: FAQ - PET

PET – Manufacturing process of polyethylene Terephtalate (PET) :

Polyethylene Terephthalate (PET) is one of the major polymers produced worldwide representing about 18 % of world polymer production and comes in third after Polyethylene and Polypropylene. The main downstream industries based on PET are production of polyester fibers, accounting for around 65% of global consumption, and PET bottle resins consuming around 30%.
PET is produced from high purity ethylene glycol (EG) and Terephthalic acid (TPA).  All PET resin manufacture processes are using the same reaction path as shown in the figure bellow :

The conventional PET process consists of two discrete plant sections. The first part consists of melt phase reaction used to produce copolymers with an intrinsic viscosity (IV) suitable for textile applications. But when very high molecular weights are desired, as is the case for bottle grade PET resins, the polymerization may be carried out in stages. The traditional Buhler process integrates four typical stages for producing bottle grade PET : crystallization, annealing, solid state polymerization (SSP) and cooling. New technologies are currently replacing this design with a tendency to reduce the number of units involved
and thus the global process cost.

A radical approach that is rapidly becoming more and more employed is Eastman IntegRex technology (illustrated in figure 2). The main unit is a tubular reactor that leads to a significant reduction of energy, raw materials consumptions, operation costs and capital costs.

Example pf Eastman IntegRex PET technology

Figure 2. Eastman IntegRex manufacturing technology

Posted in: FAQ - PET

PET – Recommended valves :

To prevent polymerization of the fluid, the valves should mostly be equipped with heating jacket and resist severe corrosion.

Posted in: FAQ - PET

Leaflet PET,PBT,PTA – pdf